Causes and Solutions of Bad Surface Coating Formed by Electrostatic Powder Spraying
Causes and Solutions of Bad Surface Coating Formed by Electrostatic Powder Spraying
The basic principle of electrostatic spraying Powder electrostatic spraying is based on the principle of high-voltage electrostatic corona electric field. The high-voltage negative electrode is connected to the metal guide ring of the spray gun head, and the sprayed workpiece is grounded to form a positive electrode. A strong electrostatic electric field is formed between the spray gun and the aluminum profile. When the compressed air is used as a carrier to transport the powder coating from the powder supply tank to the spray gun guide ring through the powder feeding pipe, the corona discharge generated by the connection between the guide ring and the high-voltage negative electrode generates a dense negative charge nearby. it. The powder is negatively charged and enters an electrostatic field with high electric field strength. Under the dual action of electrostatic force and carrier gas, the powder evenly flies to the grounded workpiece, forming a powder coating with uniform thickness on the surface of the aluminum profile. After heating and curing, it is converted into a coating film with certain corrosion resistance
2. Causes and solutions of poor coating surface
1. Insufficient gloss of the coating film: the baking time is too long during curing; the temperature is too high; other harmful gases are mixed in the baking process; the surface of the workpiece is too rough; the pretreatment method is not selected properly.
2. Discoloration of the coating film: repeated baking several times; other gases mixed in the oven; excessive baking during the curing process.
3. Orange peel on the surface of the coating film: uneven thickness of the spray layer; poor powder atomization and powder accumulation in the spray gun; low curing temperature; wet powder, too coarse powder particles; poor grounding of the workpiece; too high baking temperature; too thin coating film .
4. Coating concave holes: improper handling, unclean degreasing; pollution source, compressed air degreasing, incomplete dehydration; uneven surface of workpiece; contamination by dust or other impurities.
5. There are air bubbles in the coating film: After the surface of the workpiece is treated, the moisture is not completely dried, leaving pre-treatment residue; the degreasing and rust removal is not complete; the bottom volatiles are not cleaned; the surface of the workpiece has pores; the powder coating is too thick.
6. Uneven coating film: uneven powder coating; too close distance between spray gun and workpiece; unstable high pressure output.
7. The impact strength and adhesion of the coating film are poor: the phosphating film is too thick; the curing temperature is too low, the time is too short, and the curing is incomplete; the bottom metal is not cleaned; the adhesion of the coated workpiece will decrease after soaking in water.
8. Coating pinholes: there are foreign objects and residual oil in the air; the voltage of the spray gun is too high, causing the coating to break down; the distance between the spray gun and the workpiece is too close, causing the coating to crack; the coating is too thin; the coating film is not completely cured.
9. There is a small amount of sand on the surface of the coating film: the spraying is blocked or the airflow is not good; the atomization of the spray gun is not good; there is powder dripping in the powder spraying room; other debris contaminates the surface of the workpiece.
10. Coating peeling: poor surface treatment of the workpiece, incomplete degreasing and rust removal; insufficient output voltage of the high-voltage electrostatic generator; poor grounding of the workpiece; excessive air pressure during the milling process;
11. Uneven powder supply: the powder supply pipe or the powder spraying pipe is blocked, and the powder adheres and hardens at the nozzle; the air pressure is insufficient and the pressure is unstable; the air compressor is mixed with oil or water; the powder supply fluidization is unstable. There is too little powder in the powder feeder; the powder supply pipe is too long, and the resistance increases when the powder flows.
12. Poor adsorption of flying powder: There is no high-voltage short circuit phenomenon in the electrostatic generator; the workpiece is poorly grounded; the air pressure is too high; the air duct in the recovery device is blocked.
13. Small amount of powder spraying: insufficient air pressure and insufficient air volume; too high air pressure, and the mixture ratio of powder and flow material is too high; moisture and oil are mixed in the air space; the spray gun head is partially blocked.
14. The powder spraying pipe is blocked: due to the material of the powder spraying pipe, the powder is easy to adhere to the pipe wall; the output pipe is heated, causing the powder in the pipe to agglomerate; the powder conveying pipe is bent and deformed; the powder is mixed with relatively solid particles.
3. Conclusion
The drawbacks that often appear in the use of powder coatings are sudden. In addition to the bad reasons that are more likely to occur in the production of the above-mentioned processes, there are many factors that affect the quality of the coating surface, which need to be continuously researched, explored and summarized in the production. , Improve process conditions, avoid coating defects as much as possible, and improve the quality of sprayed products. In short, proper process specification and operation in strict accordance with the process specification are important conditions for obtaining high-quality coating pretreatment effect. In the process of coating production, it is necessary to formulate advanced and feasible process specifications, and more importantly, let the operator truly grasp the key points and difficulties, strictly implement and strengthen management, avoid coating defects, and improve spray products. A practical and effective quality method.